  2. Soldering - Wikipedia

    en.wikipedia.org/wiki/Soldering

    Extra-easy solder contains 56% silver and has a melting point of 618 °C (1,145 °F). Extra-hard solder has 80% silver and melts at 740 °C (1,370 °F). If multiple joints are needed, then the jeweler will start with hard or extra-hard solder and switch to lower-temperature solders for later joints. Silver solder is somewhat absorbed by the ...

  3. Solder - Wikipedia

    en.wikipedia.org/wiki/Solder

    Soldering performed using alloys with a melting point above 450 °C (840 °F; 720 K) is called "hard soldering", "silver soldering", or brazing. In specific proportions, some alloys are eutectic — that is, the alloy's melting point is the lowest possible for a mixture of those components, and coincides with the freezing point.

  4. Solder alloys - Wikipedia

    en.wikipedia.org/wiki/Solder_alloys

    Soldering copper pipes using a propane torch and a lead-free solder. Solder is a metallic material that is used to connect metal workpieces. The choice of specific solder alloys depends on their melting point, chemical reactivity, mechanical properties, toxicity, and other properties.

  5. Silver soldering - Wikipedia

    en.wikipedia.org/?title=Silver_soldering&redirect=no

    What links here; Related changes; Upload file; Special pages; Permanent link; Page information; Cite this page; Get shortened URL; Download QR code

  6. Flux (metallurgy) - Wikipedia

    en.wikipedia.org/wiki/Flux_(metallurgy)

    Brazing (sometimes known as silver soldering or hard soldering) requires a higher temperature than soft soldering (> 450 °C). As well as removing existing oxides, rapid oxidation of the metal at the elevated temperatures has to be avoided.

  7. Tin-silver-copper - Wikipedia

    en.wikipedia.org/wiki/Tin-silver-copper

    Tin-silver-copper (Sn-Ag-Cu, also known as SAC), is a lead-free alloy commonly used for electronic solder. It is the main choice for lead-free surface-mount technology (SMT) assembly in the industry, [ 1 ] as it is near eutectic , with adequate thermal fatigue properties, strength, and wettability. [ 2 ]

  8. Brazing - Wikipedia

    en.wikipedia.org/wiki/Brazing

    Silver brazing may cause defects in certain alloys, e.g. stress-induced inter-granular cracking in copper-nickel. One special silver brazing method is called pinbrazing or pin brazing. It has been developed especially for connecting cables to railway track or for cathodic protection installations. The method uses a silver- and flux-containing ...

  9. Whisker (metallurgy) - Wikipedia

    en.wikipedia.org/wiki/Whisker_(metallurgy)

    Silver whiskers growing out of surface-mount resistors Metal whiskering is a phenomenon that occurs in electrical devices when metals form long whisker-like projections over time. Tin whiskers were noticed and documented in the vacuum tube era of electronics early in the 20th century in equipment that used pure, or almost pure, tin solder in ...