Results From The WOW.Com Content Network
The Rockwell scale is a hardness scale based on indentation hardness of a material. The Rockwell test measures the depth of penetration of an indenter under a large load (major load) compared to the penetration made by a preload (minor load). [1] There are different scales, denoted by a single letter, that use different loads or indenters.
ISO 18265: "Metallic materials — Conversion of hardness values" (2013) ASTM E140-12B(2019)e1: "Standard Hardness Conversion Tables for Metals Relationship Among Brinell Hardness, Vickers Hardness, Rockwell Hardness, Superficial Hardness, Knoop Hardness, Scleroscope Hardness, and Leeb Hardness" (2019)
The Brinell hardness is designated by the most commonly used test standards (ASTM E10-14 [2] and ISO 6506–1:2005) as HBW (H from hardness, B from brinell and W from the material of the indenter, tungsten (wolfram) carbide). In former standards HB or HBS were used to refer to measurements made with steel indenters.
A6, a grade of tool steel which air-hardens at a relatively low temperature (approximately the same temperature as oil-hardening grades) and is dimensionally stable. Therefore, it is commonly used for dies, forming tools, and gauges that do not require extreme wear resistance but do need high stability.
International Organization for Standardization ISO/TS 4949:2016; European standards – EN 10027; Japanese steel grades : Japanese Industrial Standards (JIS) standard and NK standard; Germany steel grades : DIN standard; China steel grades : GB standard; Czech steel grades : ČSN standard; Russia steel grades : GOST standard; Spain steel grades ...
The Vickers test can be used for all metals and has one of the widest scales among hardness tests. The unit of hardness given by the test is known as the Vickers Pyramid Number ( HV ) or Diamond Pyramid Hardness ( DPH ).
Then, the bottom of the gauge block is observed (through the optical flat) for oil or color. For Federal Grades 0.5, 1, and 2 and ISO grades K, 00, and 0 no oil or color should be visible under the gauge block. For Federal Grade 3 and ISO grades 1 and 2, no more than 20% of the surface area should show oil or color.
UNS S17400 is ASTM grade 630, Cr-Ni 17-4PH precipitation hardened stainless steel; UNS S30400 is SAE 304, Cr/Ni 18/10, Euronorm 1.4301 stainless steel; UNS S31600 is SAE 316; UNS S31603 is 316L, a low carbon version of 316. The digits "03" were assigned since the maximum allowed carbon content is 0.03%; UNS C90300 is CDA 903