where I is the moment of inertia of the beam cross-section and c is the distance of the top of the beam from the neutral axis (see beam theory for more details). For a beam of cross-sectional area a and height h , the ideal cross-section would have half the area at a distance h / 2 above the cross-section and the other half at a ...
ASTM A992 steel is a structural steel alloy often used in the US for steel wide-flange and I beams. Like other carbon steels, the density of ASTM A992 steel is approximately 7850 kg/m 3 (0.2836 lb/in 3). ASTM A992 steel has the following minimum mechanical properties, according to ASTM specification A992/A992M.
The RV-3 uses a NACA 23012 airfoil on a constant chord wing. Construction is semi-monocoque of predominantly 2024-T3 aluminum sheet. The wings are built around an aluminum I-beam spar with a lighter rear spar. The aircraft has plain flaps operated by a handle. The main landing gear is attached directly to the welded steel engine mount and ...
ASTM B221: Standard Specification for Aluminum and Aluminum-Alloy Extruded Bars, Rods, Wire, Profiles, and Tubes; ASTM B308/308M: Standard Specification for Aluminum-Alloy 6061-T6 Standard Structural Profiles; ASTM B483: Standard Specification for Aluminum and Aluminum-Alloy Drawn Tube and Pipe for General Purpose Applications
Automotive arc welding (aluminum) AWS D9.1: Sheet metal welding AWS D10.10: Heating practices for pipe and tube AWS D10.11: Root pass welding for pipe AWS D10.12: Pipe welding (mild steel) AWS D10.13: Tube brazing (copper) AWS D10.18: Pipe welding (stainless steel) AWS D11.2: Welding (cast iron) AWS D14.1: Industrial mill crane welding AWS D14.3
Typical material properties for 6005A aluminum alloy include: [2] Density: 2.71 g/cm 3, or 169 lb/ft 3. Electrical Conductivity: 47 to 50% IACS. Young's modulus: 70 GPa, or 10 Msi. Ultimate tensile strength: 190 to 300 MPa, or 28 to 44 ksi. Yield strength: 100 to 260 MPa, or 15 to 38 ksi. Thermal Conductivity: 180 to 190 W/m-K.