Steel is between 0 and 2.06 mass percent of carbon. Cast iron is between 2.06 and 6.67%. Black lines indicate the metastable Fe/Fe3Cphase, red is the stable Fe/Carbon phase This diagram is for illustrative purposes only, and is not thermodynamically accurate.
Low-pressure phase diagram of pure iron. BCC is body centered cubic and FCC is face-centered cubic. Iron-carbon eutectic phase diagram, showing various forms of Fe x C y substances. Iron allotropes, showing the differences in structure. The alpha iron (α-Fe) is a body-centered cubic (BCC) and the gamma iron (γ-Fe) is a face-centered cubic (FCC).
English: Iron-carbon binary phase diagram: metastable (cementite) in plain line; stable (graphite) in dashed line. Caption: Fe 3 C: cementite (iron carbide); L: liquid; α: ferrite (alpha iron), body-centered cubic; δ: delta-iron, body-centered cubic; γ: austenite (gamma iron), face-centered cubic; solvus A 1: lower limit of existence of ...
The iron-carbon phase diagram. While cementite is thermodynamically unstable, eventually being converted to austenite (low carbon level) and graphite (high carbon level) at higher temperatures, it does not decompose on heating at temperatures below the eutectoid temperature (723 °C) on the metastable iron-carbon phase diagram.
Iron-carbon phase diagram. α-Iron is a fairly soft metal that can dissolve only a small concentration of carbon (no more than 0.021% by mass at 910 °C). [133] Austenite (γ-iron) is similarly soft and metallic but can dissolve considerably more carbon (as much as 2.04% by mass at 1146 °C).
Iron-carbon phase diagram, showing the conditions under which austenite (γ) is stable in carbon steel. Allotropes of iron; alpha iron and gamma iron. Austenite, also known as gamma-phase iron (γ-Fe), is a metallic, non-magnetic allotrope of iron or a solid solution of iron with an alloying element. [1]
Discover the latest breaking news in the U.S. and around the world — politics, weather, entertainment, lifestyle, finance, sports and much more.
Pearlite occurs at the eutectoid of the iron-carbon phase diagram (near the lower left). Pearlite is a two-phased , lamellar (or layered) structure composed of alternating layers of ferrite (87.5 wt%) and cementite (12.5 wt%) that occurs in some steels and cast irons .