Search results
Results From The WOW.Com Content Network
Cast iron is between 2.06 and 6.67%. Black lines indicate the metastable Fe/Fe3Cphase, red is the stable Fe/Carbon phase This diagram is for illustrative purposes only, and is not thermodynamically accurate.
Low-pressure phase diagram of pure iron. BCC is body centered cubic and FCC is face-centered cubic. Iron-carbon eutectic phase diagram, showing various forms of Fe x C y substances. Iron allotropes, showing the differences in structure. The alpha iron (α-Fe) is a body-centered cubic (BCC) and the gamma iron (γ-Fe) is a face-centered cubic (FCC).
Iron-carbon phase diagram, showing the iron-carbon phase diagram (near the lower left). In iron and steel metallurgy, ledeburite is a mixture of 4.3% carbon in iron and is a eutectic mixture of austenite and cementite. Ledeburite is not a type of steel as the carbon level is too high although it may occur as a separate constituent in
Iron-carbon phase diagram. α-Iron is a fairly soft metal that can dissolve only a small concentration of carbon (no more than 0.021% by mass at 910 °C). [133] Austenite (γ-iron) is similarly soft and metallic but can dissolve considerably more carbon (as much as 2.04% by mass at 1146 °C).
The iron-carbon phase diagram. While cementite is thermodynamically unstable, eventually being converted to austenite (low carbon level) and graphite (high carbon level) at higher temperatures, it does not decompose on heating at temperatures below the eutectoid temperature (723 °C) on the metastable iron-carbon phase diagram.
English: Iron-carbon binary phase diagram: metastable (cementite) in plain line; stable (graphite) in dashed line. Caption: Fe 3 C: cementite (iron carbide); L: liquid; α: ferrite (alpha iron), body-centered cubic; δ: delta-iron, body-centered cubic; γ: austenite (gamma iron), face-centered cubic; solvus A 1: lower limit of existence of ...
Hexaferrum and epsilon iron (ε-Fe) are synonyms for the hexagonal close-packed (HCP) phase of iron that is stable only at extremely high pressure. A 1964 study at the University of Rochester mixed 99.8% pure α-iron powder with sodium chloride , and pressed a 0.5-mm diameter pellet between the flat faces of two diamond anvils.
Pearlite occurs at the eutectoid of the iron-carbon phase diagram (near the lower left). Pearlite is a two-phased , lamellar (or layered) structure composed of alternating layers of ferrite (87.5 wt%) and cementite (12.5 wt%) that occurs in some steels and cast irons .