When.com Web Search

Search results

  1. Results From The WOW.Com Content Network
  2. 2017 aluminium alloy - Wikipedia

    en.wikipedia.org/wiki/2017_aluminium_alloy

    Print/export Download as PDF; ... Aluminum: 91.5 - 95.5 Copper: 3.5 - 4.5 Iron: ... Tensile strength (annealed) 179 MPa Yield strength (annealed) 69 MPa

  3. 7050 aluminium alloy - Wikipedia

    en.wikipedia.org/wiki/7050_aluminium_alloy

    It has high toughness, high strength. It has high stress corrosion cracking resistance. [1] It has electric conductivity of value having 40 percent of copper. [2] 7050 aluminium is known as a commercial aerospace alloy. [3]

  4. 6005A aluminium alloy - Wikipedia

    en.wikipedia.org/wiki/6005A_aluminium_alloy

    Typical material properties for 6005A aluminum alloy include: [2] Density: 2.71 g/cm 3, or 169 lb/ft 3. Electrical Conductivity: 47 to 50% IACS. Young's modulus: 70 GPa, or 10 Msi. Ultimate tensile strength: 190 to 300 MPa, or 28 to 44 ksi. Yield strength: 100 to 260 MPa, or 15 to 38 ksi. Thermal Conductivity: 180 to 190 W/m-K.

  5. 7178 aluminium alloy - Wikipedia

    en.wikipedia.org/wiki/7178_aluminium_alloy

    Download as PDF; Printable version ... 7178 aluminum alloy is wrought alloy. It has high ... Ultimate Tensile Strength [4] 607 MPa Tensile Yield Strength [4] 538 MPa ...

  6. 6013 aluminium alloy - Wikipedia

    en.wikipedia.org/wiki/6013_aluminium_alloy

    Download as PDF; Printable version; In other projects ... Aluminum, Al 94.8-97.8 Magnesium, Mg ... Tensile strength ≥ 392 MPa Yield strength

  7. 5086 aluminium alloy - Wikipedia

    en.wikipedia.org/wiki/5086_aluminium_alloy

    Unhardened 5086 has a yield strength of 120 MPa (17 ksi) and ultimate tensile strength of 260 MPa (38 ksi) from −28 to 100 °C (−18 to 212 °F). At cryogenic temperatures it is slightly stronger: at −196 °C (−321 °F), yield of 130 MPa (19 ksi) and ultimate tensile strength of 380 MPa (55 ksi); above 100 °C (212 °F) its strength is reduced.

  8. 7068 aluminium alloy - Wikipedia

    en.wikipedia.org/wiki/7068_aluminium_alloy

    7068 alloy is a 7000 series aluminium-zinc alloy registered with the US Aluminium Association and produced to AMS 4331 (chemical composition and mechanical properties) and AMS 2772 (heat treatment). 7068 alloy ‘A’ and ‘B’ tensile data and fatigue properties have been ratified for inclusion in MIL Handbook 5 / MMPDS.

  9. 7075 aluminium alloy - Wikipedia

    en.wikipedia.org/wiki/7075_aluminium_alloy

    T6 temper 7075 has an ultimate tensile strength of 510–540 MPa (74,000–78,000 psi) and yield strength of at least 430–480 MPa (63,000–69,000 psi). It has a failure elongation of 5–11%. [9] The T6 temper is usually achieved by homogenizing the cast 7075 at 450 °C for several hours, quenching, and then ageing at 120 °C for 24 hours.

  1. Related searches aluminum yield strength chart pdf free template superkids printable coloring pages