The pavement condition index (PCI) is a numerical index between 0 and 100, which is used to indicate the general condition of a pavement section.The PCI is widely used in transportation civil engineering [1] and asset management, and many municipalities use it to measure the performance of their road infrastructure and their levels of service. [2]
The CBR is expressed as a percentage of the actual load causing the penetrations of 2.5 mm or 5.0 mm to the standard loads on crushed stone. A load penetration curve is drawn. The load values on standard crushed stones are 1,370 kgf (13.44 kN) and 2,055 kgf (20.15 kN) at 2.5 mm and 5.0 mm penetrations respectively. [citation needed]
The PASER scale is a 1-10 rating system for road pavement condition developed by the University of Wisconsin-Madison Transportation Information Center. PASER uses visual inspection to evaluate pavement surface conditions. When assessed correctly, PASER ratings provide a basis for comparing the quality of roadway segments. [1]
Many other agencies have adopted the California pavement design method, and specify R-Value testing for subgrade soils and road aggregates. The test method states: The R-value of a material is determined when the material is in a state of saturation such that water will be exuded from the compacted test specimen when a 16.8 kN load (2.07 MPa ...
FWD data is most often used to calculate stiffness-related parameters of a pavement structure. The process of calculating the elastic moduli of individual layers in a multi-layer system (e.g. asphalt concrete on top of a base course on top of the subgrade) based on surface deflections is known as "backcalculation", as there is no closed-form solution.
Pavement performance modeling or pavement deterioration modeling is the study of pavement deterioration throughout its life-cycle. [ 1 ] [ 2 ] The health of pavement is assessed using different performance indicators.
The frequency of the suspension response at the golden-car simulation speed also determines the final IRI ride value. The IRI sensitivity is focused on wavelengths between 0.82 and nearly 200-feet (0.25 to 61 meters). Although, if any wavelengths are equal to 7.9 or 50 feet (2.4 or 15.2 meters) the IRI values are weighted higher. [2]