In direct extrusion the billet is pushed through the die with ram pressure, whereas in indirect extrusion a die moves relative to the container. Rule based analysis of extrusion process would help to determine a set of rules essential for consideration while designing a product, or even during cost estimation of a product. Some rules are ...
ASTM B221: Standard Specification for Aluminum and Aluminum-Alloy Extruded Bars, Rods, Wire, Profiles, and Tubes; ASTM B308/308M: Standard Specification for Aluminum-Alloy 6061-T6 Standard Structural Profiles; ASTM B483: Standard Specification for Aluminum and Aluminum-Alloy Drawn Tube and Pipe for General Purpose Applications
Typical material properties for 6005A aluminum alloy include: [2] Density: 2.71 g/cm 3, or 169 lb/ft 3. Electrical Conductivity: 47 to 50% IACS. Young's modulus: 70 GPa, or 10 Msi. Ultimate tensile strength: 190 to 300 MPa, or 28 to 44 ksi. Yield strength: 100 to 260 MPa, or 15 to 38 ksi. Thermal Conductivity: 180 to 190 W/m-K.
6063 is the most common alloy used for aluminium extrusion. It allows complex shapes to be formed with very smooth surfaces fit for anodizing and is popular for visible architectural applications such as window frames, door frames, roofs, and sign frames. [ 3 ]
A horizontal hydraulic press for hot aluminum extrusion (loose dies and scrap visible in foreground) There are many different variations of extrusion equipment. They vary by four major characteristics: [1] Movement of the extrusion with relation to the ram. If the die is held stationary and the ram moves towards it then it is called "direct ...
In steel extrusions, the depth of an indentation should be no greater than its width at its narrowest point. This is necessary to provide sufficient strength in the tongue portion of the extruding die. In copper alloys, magnesium, and aluminum, the depth of an indentation may be greater since extrusion pressures are lower.
ASTM B 221: Standard Specification for Aluminium and Aluminium-Alloy Extruded Bars, Rods, Wire, Profiles, and Tubes; EN 573-3: Aluminium and aluminium alloys. Chemical composition and form of wrought products. Chemical composition and form of products; EN 755-2: Aluminium and aluminium alloys. Extruded rod/bar, tube and profiles. Mechanical ...
6105 aluminium alloy is an alloy in the wrought aluminium-magnesium-silicon family (6000 or 6xxx series). It is one of the least common of the alloys in this series. While most wrought aluminium alloys are covered by multiple standards (from any mixture of ASTM, EN, ISO, and national standard bodies), 6105 is only dealt with in ASTM B221: Standard Specification for Aluminum and Aluminum-Alloy ...