Search results
Results From The WOW.Com Content Network
iron: ferrite, ferritic steel; iron: austenite, austenitic steel; iron carbide: cementite, Fe3C. It shows a eutectic and a eutectoid; these phases crystallise as a stacking of fine strips of pure phases (iron and cementite) in case of the eutectoid, or a pure iron containing small balls of cementite for the eutectic.
The iron-carbon phase diagram. While cementite is thermodynamically unstable, eventually being converted to austenite (low carbon level) and graphite (high carbon level) at higher temperatures, it does not decompose on heating at temperatures below the eutectoid temperature (723 °C) on the metastable iron-carbon phase diagram.
English: Iron-carbon binary phase diagram: metastable (cementite) in plain line; stable (graphite) in dashed line. Caption: Fe 3 C: cementite (iron carbide); L: liquid; α: ferrite (alpha iron), body-centered cubic; δ: delta-iron, body-centered cubic; γ: austenite (gamma iron), face-centered cubic; solvus A 1: lower limit of existence of ...
Low-pressure phase diagram of pure iron. BCC is body centered cubic and FCC is face-centered cubic. Iron-carbon eutectic phase diagram, showing various forms of Fe x C y substances. Iron allotropes, showing the differences in structure. The alpha iron (α-Fe) is a body-centered cubic (BCC) and the gamma iron (γ-Fe) is a face-centered cubic (FCC).
The phase diagram shows, in pressure–temperature space, the lines of equilibrium or phase boundaries between the three phases of solid, liquid, and gas. The curves on the phase diagram show the points where the free energy (and other derived properties) becomes non-analytic: their derivatives with respect to the coordinates (temperature and ...
A phase diagram for a fictitious binary chemical mixture (with the two components denoted by A and B) used to depict the eutectic composition, temperature, and point. ( L denotes the liquid state.) A eutectic system or eutectic mixture ( / j uː ˈ t ɛ k t ɪ k / yoo- TEK -tik ) [ 1 ] is a type of a homogeneous mixture that has a melting point ...
Pearlite occurs at the eutectoid of the iron-carbon phase diagram (near the lower left). Pearlite is a two-phased , lamellar (or layered) structure composed of alternating layers of ferrite (87.5 wt%) and cementite (12.5 wt%) that occurs in some steels and cast irons .
An iron-carbon phase diagram showing the conditions necessary to form different phases An incandescent steel workpiece in a blacksmith's art. Iron is commonly found in the Earth's crust in the form of an ore, usually an iron oxide, such as magnetite or hematite.