[7] 420A (420J1) and 420B (420J2) are economical, highly corrosion-resistant stainless steel grades. Knife manufacturers use this material in budget knives, also in diving knives due to its high corrosion resistance. [7] 440 series has three types: 440A, 440B, and 440C. 440A is a relatively low-cost, highly corrosion-resistant stainless steel.
In general: the higher PREN-value, the more resistant is the stainless steel to localized pitting corrosion by chloride. PREN is frequently specified when stainless steels will be exposed to seawater or other high chloride solutions. In some instances stainless steels with PREN-values > 32 may provide useful resistance to pitting corrosion in ...
In 2009, Crucible Steel introduced an update to CPM-S30V to meet the needs of renowned knife maker Chris Reeve that they called CPM-S35VN. The addition of 0.5% Niobium, and reductions in both Carbon (from 1.45% to 1.40%) and Vanadium (from 4% to 3%) produced an alloy with 25% increase in measured Charpy V-notch toughness over S30V (Crucible claims 15-20% improvement).
This metal is commonly used instead of 300 series stainless steels in high temperature and low pH applications in food processing. For example, tomato juice will corrode 316L stainless steel at pasteurization temperatures of 100 °C (210 °F). AL-6XN will better resist this corrosion while still offering the beneficial properties of stainless ...
Stainless steel, also known as inox, corrosion-resistant steel (CRES), and rustless steel, is an iron-based alloy containing a minimum level of chromium that is resistant to rusting and corrosion. Stainless steel's resistance to corrosion results from the 10.5%, or more, chromium content which forms a passive film that can protect the material ...
The unshaded bars indicate the location on the chart of those steels when in acidic/stagnant water ( like in the bilge ), where crevice-corrosion happens. Notice how the *same* steel has much different galvanic-series location, depending on the electrolyte it's in, making prevention of corrosion .. more difficult.