Search results
Results From The WOW.Com Content Network
The weight of an asphalt pavement depends upon the aggregate type, the bitumen, and the air void content. An average example in the United States is about 112 pounds per square yard, per inch of pavement thickness. [21]
The weight designations originated with organic base felt weighing 15 or 30 pounds per 100 sq. ft. (6.8 kg or 14 kg per 9.3 m 2). However, modern base felts are made of lighter-weight fibre, so the weight designations, though common colloquially, are no longer literally accurate. [ 2 ]
Bituminous geomembrane (BGM) is a type of geomembrane consisting of a reinforcing geotextile to provide mechanical strength and elastomeric bitumen (often called asphalt in U.S.) to provide impermeability. Other components such as sand, a glass fleece, and/or a polyester film can be incorporated into the layers of a BGM. [1]
The University of Queensland pitch drop experiment, demonstrating the viscosity of bitumen. A pitch drop experiment is a long-term experiment which measures the flow of a piece of pitch over many years. "Pitch" is the name for any of a number of highly viscous liquids which appear solid, most commonly bitumen, also known as asphalt. At room ...
Asphalt batch mix plant A machine laying asphalt concrete, fed from a dump truck. Asphalt concrete (commonly called asphalt, [1] blacktop, or pavement in North America, and tarmac or bitumen macadam in the United Kingdom and the Republic of Ireland) is a composite material commonly used to surface roads, parking lots, airports, and the core of embankment dams. [2]
Several variations of bitumen roofing felt are available. Single coverage thicknesses range from 55 to 90 pounds per square (100 sq. ft.) for single-coverage; Double coverage range from 110 to 140 pounds per square. [4] Fibre content: mixed rag fibre - lowest cost, shortest life; all plastic fibres; fibreglass - longest lived; Bitumen:
The stone skeleton is filled with a mastic of bitumen and filler to which fibres are added to provide adequate stability of bitumen and to prevent drainage of binder during transport and placement. Typical SMA composition consists of 70−80% coarse aggregate, 8−12% filler, 6.0−7.0% binder, and 0.3 per cent fibre.
Tar paper is used as a roofing underlayment with asphalt, wood, shake, and other roof shingles as a form of intermediate bituminous waterproofing.It is sold in rolls of various widths, lengths, and thicknesses – 3-foot-wide (0.91 m) rolls, 50 or 100 feet (15 or 30 m) long and "15 lb" (7 kg) and "30 lb" (14 kg) weights are common in the U.S. – often marked with chalk lines at certain ...