Primary cracks (Figure 1) form when the tensile stress at the outer surface of the concrete reaches the tensile strength of concrete. When a primary crack forms, the concrete in the vicinity of the crack is relieved of any tension, resulting in a stress free zone near the crack.
The steel shuttering pinches the top surface of a concrete slab due to the weight of the next slab being constructed. Concrete slabs, block walls and pipelines are susceptible to cracking during ground settlement, seismic tremors or other sources of vibration, and also from expansion and contraction during adverse temperature changes.
Concrete has a very low coefficient of thermal expansion, and as it matures concrete shrinks. All concrete structures will crack to some extent, due to shrinkage and tension. Concrete which is subjected to long-duration forces is prone to creep. The density of concrete varies, but is around 2,400 kilograms per cubic metre (150 lb/cu ft). [1]
A corrugated slab is designed when the concrete is poured into a corrugated steel tray, more commonly called decking. This steel tray improves strength of the slab, and prevents the slab from bending under its own weight. The corrugations run in one direction only. A ribbed slab gives considerably more strength in one direction. This is ...
Typical crack pattern of the alkali-silica reaction (ASR). The gel exudations through the concrete cracks have a characteristic yellow color and a high pH. The fatty aspect of the exudations imbibing the concrete porosity along the cracks is also a distinctive feature of ASR. The alkali-silica reaction as a chemical cycle process
Robert McGee, the owner of II in One, which provided concrete and rebar services for the center starting in 2021, ... In a memo, Thornton Tomasetti shared images of cracked slab and exposed rebar.