Sodium aluminate is an inorganic chemical that is used as an effective source of aluminium hydroxide for many industrial and technical applications. Pure sodium aluminate ( anhydrous ) is a white crystalline solid having a formula variously given as NaAlO 2 , NaAl(OH) 4 ( hydrated ), [ 3 ] Na 2 O·Al 2 O 3 , or Na 2 Al 2 O 4 .
Bauxite ore is usually heated in a pressure vessel along with a sodium hydroxide solution at a temperature of 150 to 200 °C (300 to 390 °F). At these temperatures, the aluminium is dissolved as sodium aluminate (the Bayer process).
The Bayer process is the principal industrial means of refining bauxite to produce alumina (aluminium oxide) and was developed by Carl Josef Bayer.Bauxite, the most important ore of aluminium, contains only 30–60% aluminium oxide (Al 2 O 3), the rest being a mixture of silica, various iron oxides, and titanium dioxide. [1]
Sodium hexafluoroaluminate is an inorganic compound with formula Na 3 Al F 6. This white solid, discovered in 1799 by Peder Christian Abildgaard (1740–1801), [4] [5] occurs naturally as the mineral cryolite and is used extensively in the industrial production of aluminium. The compound is the sodium (Na +) salt of the hexafluoroaluminate (AlF ...
A number of aluminate oxyanions are known: The simplest is the approximately tetrahedral AlO 5− 4 found in the compound Na 5 AlO 4, [2] framework AlO − 2 ions in anhydrous sodium aluminate NaAlO 2 [3] and monocalcium aluminate, CaAl 2 O 4 made up of corner-sharing {AlO 4} tetrahedra. [4] A ring anion, the cyclic Al 6 O 18−
Red mud near Stade Bauxite, an aluminium ore (Hérault department, France).The reddish colour is due to iron oxides that make up the main part of the red mud.. Red mud, now more frequently termed bauxite residue, is an industrial waste generated during the processing of bauxite into alumina using the Bayer process.
No. of Billionaires: 813 Drivers of Wealth: Technology, finance, entertainment Famous Billionaire: Elon Musk 2. China
The process produces a quantity of fluoride waste: perfluorocarbons and hydrogen fluoride as gases, and sodium and aluminium fluorides and unused cryolite as particulates. This can be as small as 0.5 kg per tonne of aluminium in the best plants in 2007, up to 4 kg per tonne of aluminium in older designs in 1974.