  2. Galvanic series - Wikipedia

    en.wikipedia.org/wiki/Galvanic_series

    The unshaded bars indicate the location on the chart of those steels when in acidic/stagnant water ( like in the bilge ), where crevice-corrosion happens. Notice how the *same* steel has much different galvanic-series location, depending on the electrolyte it's in, making prevention of corrosion .. more difficult.

  3. Galvanic corrosion - Wikipedia

    en.wikipedia.org/wiki/Galvanic_corrosion

    Galvanized mild steel cable ladder with corrosion around stainless steel bolts. All metals can be classified into a galvanic series representing the electrical potential they develop in a given electrolyte against a standard reference electrode. The relative position of two metals on such a series gives a good indication of which metal is more ...

  4. Pitting resistance equivalent number - Wikipedia

    en.wikipedia.org/wiki/Pitting_Resistance...

    In general: the higher PREN-value, the more resistant is the stainless steel to localized pitting corrosion by chloride. PREN is frequently specified when stainless steels will be exposed to seawater or other high chloride solutions. In some instances stainless steels with PREN-values > 32 may provide useful resistance to pitting corrosion in ...

  5. Stainless steel - Wikipedia

    en.wikipedia.org/wiki/Stainless_steel

    Stainless steel, also known as inox, corrosion-resistant steel (CRES), and rustless steel, is an iron-based alloy containing a minimum level of chromium that is resistant to rusting and corrosion. Stainless steel's resistance to corrosion results from the 10.5%, or more, chromium content which forms a passive film that can protect the material ...

  6. Corrosion - Wikipedia

    en.wikipedia.org/wiki/Corrosion

    Corrosion in the crevice between the tube and tube sheet (both made of type 316 stainless steel) of a heat exchanger in a seawater desalination plant. Crevice corrosion is a localized form of corrosion occurring in confined spaces (crevices), to which the access of the working fluid from the environment is limited.

  7. Alloy 20 - Wikipedia

    en.wikipedia.org/wiki/Alloy_20

    Alloy 20 is an austenitic stainless steel containing less than 50% iron developed for applications involving sulfuric acid.Its corrosion resistance also finds other uses in the chemical, petrochemical, power generation, and plastics industries.

  8. SAE 304 stainless steel - Wikipedia

    en.wikipedia.org/wiki/SAE_304_stainless_steel

    For more severe corrosion conditions, when 304 stainless steel is too sensitive to pitting or crevice corrosion by chlorides or general corrosion in acidic applications, it is commonly replaced by 316 stainless steel. 304 and 302 stainless steels are subject to chloride stress fracture failure when used in tropical salt water conditions such as ...

  9. SAE steel grades - Wikipedia

    en.wikipedia.org/wiki/SAE_steel_grades

    Type 316—the second most common grade (after 304); for food and surgical stainless steel uses; alloy addition of molybdenum prevents specific forms of corrosion. It is also known as marine grade stainless steel due to its increased resistance to chloride corrosion compared to type 304. 316 is often used for building nuclear reprocessing plants.