The wood from the southern yellow pines typically has a density value between 50 and 55 lb/cu ft (0.80 and 0.88 g/cm 3) when pressure treated. Yellow pine grows across the South and Mid-Atlantic regions, from Texas to New Jersey. [7] [8]
Copper naphthenate sold for pressure treatment of wood is typically supplied as an 8% copper (as metal) concentrate for dilution to 0.5-1.5% copper (as metal) treating solutions. Copper naphthenate sold at retail for consumer use is typically a 1% or 2% copper ready-to-use solution in mineral spirits or other similar solvents.
The PTI preservative imparts very little color to the wood. Producers generally add a color agent or a trace amount of copper solution so as to identify the wood as pressure treated and to better match the color of other pressure treated wood products. The PTI wood products are very well adapted for paint and stain applications with no bleed ...
The mixture is infused into wood at high pressure. [4] In the treated wood, arsenic is believed to be in the form of chromium (III) arsenate CrAsO 4 and/or copper(II) arsenate Cu 3 (AsO 4) 2, or fairly stable chromium dimer-arsenic clusters. [4]
Wood stabilization is a series of processes which use pressure and/or vacuum to impregnate wood ... Poplar treated with MMA increased specimen density by 2 ...