  2. Threaded rod - Wikipedia

    en.wikipedia.org/wiki/Threaded_rod

    Metric threaded rods are marked on the end with a color code to define the ISO strength class. The color codes are: [9] Unmarked — 4.6 class (tensile strength = 400 N/mm 2, yield strength 240 N/mm 2) Yellow — 8.8 class (800 N/mm 2, 640 N/mm 2) Green — A2 stainless steel (304) Red — A4 stainless steel (316) White — 10.9 class (1000 N ...

  3. ASTM A354 - Wikipedia

    en.wikipedia.org/wiki/ASTM_A354

    This standard defines the properties for fasteners up to 4 inches in diameter. They are not to be used in applications where they are tensioned to more than 50% of their tensile strength. In those applications structural heavy hex bolts are to be used, as defined by ASTM A490, even though they have the same strength. [1] [2]

  4. Tension member - Wikipedia

    en.wikipedia.org/wiki/Tension_member

    [3] [4] [5] The design of tension members requires careful analysis of potential failure modes, specifically yielding (excessive deformation) and fracture, which are referred to as limit states. The governing limit state is the one that results in the lowest design strength, as it dictates the member's capacity and prevents structural failure.

  5. ASTM A325 - Wikipedia

    en.wikipedia.org/wiki/ASTM_A325

    ASTM A325 is an ASTM International standard for heavy hex structural bolts, titled Standard Specification for Structural Bolts, Steel, Heat Treated, 120/105 ksi Minimum Tensile Strength. It defines mechanical properties for bolts that range from 1 ⁄ 2 to 1 + 1 ⁄ 2 inches (13 to 38 mm) in diameter. [1]

  6. Rebar - Wikipedia

    en.wikipedia.org/wiki/Rebar

    ASTM A706 Gr. 60 is an example of a controlled property range material specification which has a minimum yield strength of 60 ksi (420 MPa), maximum yield strength of 78 ksi (540 MPa), minimum tensile strength of 80 ksi (550 MPa) and not less than 1.25 times the actual yield strength, and minimum elongation requirements that vary by bar size.

  7. Tie rod - Wikipedia

    en.wikipedia.org/wiki/Tie_rod

    The working strength of a tie rod is the product of the allowable working stress and the rod's minimum cross-sectional area. If threads are cut into a cylindrical rod, that minimum area occurs at the root of the thread. Often rods are upset (made thicker at the ends) so that the tie rod does not become weaker when threads are cut into it.

  8. Steel grades - Wikipedia

    en.wikipedia.org/wiki/Steel_grades

    The next set of 3 digits gives the steel's minimum yield strength. So S355 has a minimum yield strength of 355 MPa for the smallest thickness range covered by the relevant standard – i.e. EN10025. [2] Below is a table indicating the most common application codes.

  9. Cold-formed steel - Wikipedia

    en.wikipedia.org/wiki/Cold-formed_steel

    Yield Strength Fy (ksi) Tensile Strength Fu (ksi) Fu / Fy Minimum Elongation (%) in 2-in. Gage Length Carbon structural steel A36 36 58-80 1.61 23 A36 50 70 1.4 21 High-strength low-alloy Structural steel A242 46 67 1.46 21 Low and intermediate tensile strength carbon steel plates A283 A 24 45-60 1.88 30 B 27 50-65 1.85 28 C 30 55-75 1.83 25 D 33