A2 stainless steel outside the US, in accordance with ISO 3506 for fasteners. [4] 18/8 and 18/10 stainless steel (also written 18-8 and 18-10) in the commercial tableware and fastener industries. SUS304 the Japanese JIS G4303 equivalent grade. 1.4301, the EN 10088 equivalent. [5] 06Cr19Ni10 and ISC S30408, the equivalent in Chinese GB/T 20878 ...
904L is an austenitic stainless steel.It is softer than 316L, [1] [2] and its molybdenum addition gives it superior resistance to localized attack (pitting and crevice corrosion) by chlorides and greater resistance reducing acids; in particular, its copper addition gives it useful corrosion resistance to all concentrations of sulfuric acid.
Press fittings with appropriate and region-specific certification may be used for gas lines. Stainless steel and carbon steel press fittings can withstand up to 16 bars of pressure. A disadvantage of press fittings is the dead space between the pipe and the fitting, which can possibly rule out use for beverage and food applications.
Stainless steel, also known as inox, corrosion-resistant steel (CRES), and rustless steel, is an iron-based alloy containing a minimum level of chromium that is resistant to rusting and corrosion. Stainless steel's resistance to corrosion results from the 10.5%, or more, chromium content which forms a passive film that can protect the material ...
Type 304—the most common grade; the classic 18/8 (18% chromium, 8% nickel) stainless steel. Outside of the US it is commonly known as "A2 stainless steel", in accordance with ISO 3506 (not to be confused with A2 tool steel). [6] The Japanese equivalent grade of this material is SUS304.
UNS K11547 is T2 tool steel; UNS S17400 is ASTM grade 630, Cr-Ni 17-4PH precipitation hardened stainless steel; UNS S30400 is SAE 304, Cr/Ni 18/10, Euronorm 1.4301 stainless steel; UNS S31600 is SAE 316; UNS S31603 is 316L, a low carbon version of 316. The digits "03" were assigned since the maximum allowed carbon content is 0.03%; UNS C90300 ...