When testing wood in lumber form, the Janka test is always carried out on wood from the tree trunk (known as the heartwood), and the standard sample (according to ASTM D143) is at 12% moisture content and clear of knots. [3] The hardness of wood varies with the direction of the wood grain. Testing on the surface of a plank, perpendicular to the ...
Red oak rings in at a 1290 on the Janka scale (the higher the number, the stronger the board), and white oak comes in at 1360. Durability: Thanks to the wood’s open grain, wood stains take ...
Lignum vitae is hard and durable, and is also the densest wood traded (average dried density: ~79 lb/ft 3 or ~1,260 kg/m 3); [4] it will easily sink in water. On the Janka scale of hardness, which measures hardness of woods, lignum vitae ranks highest of the trade woods, with a Janka hardness of 4,390 lbf (compared with Olneya at 3,260 lbf, [5] African blackwood at 2,940 lbf, hickory at 1,820 ...
The wood is extremely hard, being one of the hardest woods in Northern America with a Janka hardness test of 1,700 lbf (7,560 N) [46] and specific gravity of 0.733 (733 kilograms per cubic metre or 45.7 pounds per cubic foot).
Scratch hardness. The Mohs scale of mineral hardness; The Vickers hardness test; The Brinell scale; The Janka hardness test; The Rockwell scale; The Durometer scale; The Barcol scale; The Leeb rebound hardness scale; The Rosiwal scale; The Meyer hardness test; The Knoop hardness test
Approximate wood densities of acacia species; Species Density [kg/m³] Heartwood density [kg/m³] Sapwood density [kg/m³] Acacia acuminata: 1040 [1] Acacia ...
Ironwood is a common name for many woods that have a reputation for hardness, or specifically a wood density that is denser than water (approximately 1000 kg/m 3, or 62 pounds per cubic foot), although usage of the name ironwood in English may or may not indicate a tree that yields such heavy wood.
Towards the centre of the trunk, the wood gets less hard. The wood has a Janka ball hardness of 112.5 - 154.7 kgf/cm 2 (1600 – 2200 psi), which is greater than that of oak (70.3 - 84.4 kgf/cm 2) and Douglas fir (35.9 kgf/cm 2). Coconut timber is classified according to three degrees of density: High-density timber (dermal) – hard: 600–900 ...