Steel is between 0 and 2.06 mass percent of carbon. Cast iron is between 2.06 and 6.67%. Black lines indicate the metastable Fe/Fe3Cphase, red is the stable Fe/Carbon phase This diagram is for illustrative purposes only, and is not thermodynamically accurate.
Hexaferrum and epsilon iron (ε-Fe) are synonyms for the hexagonal close-packed (HCP) phase of iron that is stable only at extremely high pressure. A 1964 study at the University of Rochester mixed 99.8% pure α-iron powder with sodium chloride , and pressed a 0.5-mm diameter pellet between the flat faces of two diamond anvils.
The primary phase of low-carbon or mild steel and most cast irons at room temperature is ferromagnetic α-Fe. [8] [9] It has a hardness of approximately 80 Brinell. [10] [11] The maximum solubility of carbon is about 0.02 wt% at 727 °C (1,341 °F) and 0.001% at 0 °C (32 °F). [12] When it dissolves in iron, carbon atoms occupy interstitial ...
2007-12-06 11:13 User A1 420×380× (344464 bytes) Steel phase diagram Iron-carbon phase diagram under atmospheric pressure This diagram is limited by pure iron on the left and by iron carbide on the right. The mains phases are: * α iron: ferrite, ferritic steel * γ iron: austenite, austeniti
English: Fe-C phase diagram of iron and carbon mixtures; showing critical temperatures for heat treatments of steels. Multilingual file, initially only in Basque, Galician, Catalan and English; but other languages can be easily added.
Iron-carbon phase diagram. α-Iron is a fairly soft metal that can dissolve only a small concentration of carbon (no more than 0.021% by mass at 910 °C). [133] Austenite (γ-iron) is similarly soft and metallic but can dissolve considerably more carbon (as much as 2.04% by mass at 1146 °C).
Iron-carbon phase diagram, showing the conditions necessary to form different phases. Distinct phases may be described as different states of matter such as gas, liquid, solid, plasma or Bose–Einstein condensate. Useful mesophases between solid and liquid form other states of matter. Distinct phases may also exist within a given state of matter.
The iron-carbon phase diagram. While cementite is thermodynamically unstable, eventually being converted to austenite (low carbon level) and graphite (high carbon level) at higher temperatures, it does not decompose on heating at temperatures below the eutectoid temperature (723 °C) on the metastable iron-carbon phase diagram.