Search results
Results From The WOW.Com Content Network
Both quantitative and qualitative tests for solderability exist. [6] The two most common testing methods are the 'dip and look' method and wetting balance analysis.In both of these tests, the soldered pieces undergo an accelerated aging process before being tested for solderability, to take into consideration the time a component was in storage prior to mounting to final assembly.
304 stainless steel is a common choice of a stainless steel. 304L stainless steel, a low-carbon variant of 304 steel, is used for ultra-high vacuum systems. 316L stainless steel a low-carbon and low-magnetic stainless steel, used in accelerator technologies. 347 stainless steel does not accept high polish. 321 stainless steel is chosen when low ...
Soldering copper pipes using a propane torch and a lead-free solder. Solder is a metallic material that is used to connect metal workpieces. The choice of specific solder alloys depends on their melting point, chemical reactivity, mechanical properties, toxicity, and other properties.
904L is an austenitic stainless steel.It is softer than 316L, [1] [2] and its molybdenum addition gives it superior resistance to localized attack (pitting and crevice corrosion) by chlorides and greater resistance reducing acids; in particular, its copper addition gives it useful corrosion resistance to all concentrations of sulfuric acid.
The galvanic series (or electropotential series) determines the nobility of metals and semi-metals.When two metals are submerged in an electrolyte, while also electrically connected by some external conductor, the less noble (base) will experience galvanic corrosion.
Chemical compatibility is a rough measure of how stable a substance is when mixed with another substance. [1] If two substances can mix together and not undergo a chemical reaction, they are considered compatible. Incompatible chemicals react with each other, and can cause corrosion, mechanical weakening, evolution of gas, fire, or other ...
Choice of developer is governed by penetrant compatibility (one can't use water-soluble or -suspendable developer with water-washable penetrant), and by inspection conditions. When using non-aqueous wet developer (NAWD) or dry powder, the sample must be dried prior to application, while soluble and suspendable developers are applied with the ...
Pitting resistance equivalent number (PREN) is a predictive measurement of a stainless steel's resistance to localized pitting corrosion based on its chemical composition. In general: the higher PREN-value, the more resistant is the stainless steel to localized pitting corrosion by chloride.