A phase diagram for a fictitious binary chemical mixture (with the two components denoted by A and B) used to depict the eutectic composition, temperature, and point. ( L denotes the liquid state.) A eutectic system or eutectic mixture ( / j uː ˈ t ɛ k t ɪ k / yoo- TEK -tik ) [ 1 ] is a type of a homogeneous mixture that has a melting point ...
It shows a eutectic and a eutectoid; these phases crystallise as a stacking of fine strips of pure phases (iron and cementite) in case of the eutectoid, or a pure iron containing small balls of cementite for the eutectic. Although it is heterogeneous, these phases behave like homogeneous pure bodies.
A binary phase diagram showing the eutectic composition, eutectic temperature, and the eutectic point: Date: 25 December 2009, 02:07 (UTC) Source: Eutektikum_new.svg;
The phase diagram shows, in pressure–temperature space, the lines of equilibrium or phase boundaries between the three phases of solid, liquid, and gas. The curves on the phase diagram show the points where the free energy (and other derived properties) becomes non-analytic: their derivatives with respect to the coordinates (temperature and ...
Low-pressure phase diagram of pure iron. BCC is body centered cubic and FCC is face-centered cubic. Iron-carbon eutectic phase diagram, showing various forms of Fe x C y substances. Iron allotropes, showing the differences in structure. The alpha iron (α-Fe) is a body-centered cubic (BCC) and the gamma iron (γ-Fe) is a face-centered cubic (FCC).
A three-component compatibility diagram will depict the stable phase of each pure component as the point at each corner of a ternary diagram. Additional points in the diagram represent other pure phases, and lines connecting pairs of these points represent compositions at which the two phases are the only phases present.
TTT diagram of isothermal transformations of a hypoeutectoid carbon steel; showing the main components obtained when cooling the steel and its relation with the Fe-C phase diagram of carbon steels. Austenite is slightly undercooled when quenched below Eutectoid temperature. When given more time, stable microconstituents can form: ferrite and ...
The temperature of the eutectic bonding procedure is dependent on the used material. The bonding happens at a specific weight-% and temperature, e.g. 370 °C at 2.85 wt-% Si for Au intermediate layer (compare to phase diagram). [5] The procedure of eutectic bonding is divided into following steps: [11] Substrate processing